Hey everyone, it’s Jake from your go-to plastic mould supplier—today we’re talking about that super annoying thing that ruins even the best-looking plastic parts: sink marks. If you’ve ever picked up a plastic phone case, a toy car, or even a kitchen storage bin and noticed that tiny, dented spot on the back, right where there’s a thick wall inside? That’s a sink mark, and trust me, I’ve gotten so many calls from clients panicking about them. Let’s break this down, no boring textbook jargon (well, maybe a little, but we’ll keep it real), and talk about how we fix them in moulds. Plastic Mould

First off, let’s keep it simple: what is a sink mark, exactly? When you inject molten plastic into a mould, it cools down, right? Thicker areas of the part take longer to cool than thin ones, kind of like how a thick slice of pizza stays hot longer than the crust. As the plastic cools and shrinks, it needs more material to fill in the gaps that form during cooling. If there’s not enough extra plastic (that’s called “packing pressure” in the mould world) or the cooling happens too fast, the thick spot shrinks inward, leaving that little dimple on the surface. Sometimes it’s barely noticeable, but other times? It’s so bad you can’t ignore it—like a water bottle that has a weird dent right where you grip it, and customers send it back immediately. I once had a client make 5,000 toy action figures that all had sink marks on their thick leg joints, and they had to toss the whole batch. Ouch.
Now, why do sink marks happen in moulds specifically? Let’s get into the nitty-gritty without making your eyes glaze over. Every plastic part has wall thickness—if it’s too uneven, that’s the #1 culprit. A part that’s 2mm thick everywhere is gonna cool evenly, but if one spot is 5mm thick? That’s where the problem starts. Another big one is packing time and pressure. When you shoot plastic into the mould, you don’t just stop when the cavity is full—you hold pressure for a bit to push more molten plastic into the shrinking areas. If you cut that step short, the thick parts can’t get enough material, and boom—sink mark. Also, plastic type matters. Some materials shrink more than others, like ABS vs. polypropylene. PP is super flexible but shrinks a ton, so it’s way more prone to sink marks if you don’t adjust the mould settings.
Here’s the good stuff: how do we avoid sink marks in moulds? This is what we do every day at our shop, so these are actual, actionable things, not just theory. First, fix the wall thickness. That’s the easiest (and most effective) fix. If your part has a thick spot, we can add a “rib” or a “draft” to thin it out, or even create a “dead space” inside the thick wall so there’s less material to shrink. For example, if you’re making a plastic gear with a thick hub, instead of making the hub solid, we can hollow it out a little—less material, less shrinkage, no sink mark. We always run simulations (that’s the software we use to test the mould before we build it) to check for thick spots before we even cut steel, which saves clients so much time and money.
Next, adjust the packing and cooling in the mould. This is where we tweak the mould design to control how plastic cools. We add “cooling channels” right next to thick areas—like tiny pipes that run through the mould steel so the plastic cools evenly. If a part has a thick boss (those little cylindrical bumps for screws, super common), we put a cooling line right next to that boss, so it cools at the same rate as the thin areas around it. We also adjust the injection pressure and time: instead of cranking pressure up all at once, we use “hold pressure” for a few extra seconds after the cavity is full. That extra pressure pushes more plastic into the shrinking thick areas, so they don’t dip inward.
Another trick we use: “gate design.” Gates are the holes where plastic flows into the mould cavity. If you have a thick part, putting a bigger gate (or multiple smaller gates) right next to the thick area lets more plastic flow there during packing, so it gets the material it needs. I had a client making a plastic remote control—their original gate was tiny, and the back had a big sink mark right over the battery compartment, which is a thick spot. We swapped the gate for a larger one on that side, adjusted the hold time, and all the sink marks were gone. They saved their whole next batch of parts.
Wait, but what if you can’t change the part design? Like, if the client already finalized the part and they can’t thin the walls? We have other hacks. One is “venting.” Adding tiny vents in the mould lets excess air and gas escape when plastic is injected, which helps the plastic flow better and fills gaps in thick areas. Sometimes we also use “hot runner” moulds—instead of plastic flowing from a cold sprue, the runner is heated, so plastic stays molten longer. That means more time to pack the thick areas, so less shrinkage. We use hot runners a lot for high-volume parts, like phone cases or appliance parts, because they cut down on waste and sink marks.
Let me be real, though—sink marks aren’t always 100% avoidable, but we can get them so small no one notices. Last year, a client came to us with a plastic outdoor table; their old mould had sink marks on the tabletop, and customers were complaining. We redesigned the mould: hollowed out the thick edges of the tabletop, added cooling channels along the edge, and used a hot runner gate. The final parts had almost zero sink marks—you had to hold them up to a light to even see a tiny, unnoticeable spot. The client was stoked, and their return rate dropped by 90%.
Now, why does this matter for you, the person ordering plastic moulds? Because sink marks aren’t just an aesthetic issue—they can weaken the part too. A sink mark is like a tiny dent in the structure; over time, that spot can crack, especially if the part is under stress, like a car panel or a medical device. So fixing sink marks isn’t just about making the part look good—it’s about making it last.
At our mould shop, we don’t just build moulds and send them out. We work with clients from the first design sketch all the way to the final part. If you have a part that’s getting sink marks, or you’re designing a new product and want to avoid them, hit us up. We’ll run those mould simulations for free, suggest tweaks to the design or mould, and make sure your parts come out perfect, no dents, no headaches.
Oh, and one quick pro tip: if you’re dealing with a part that already has a sink mark, sometimes you can fix it after moulding, but it’s way cheaper and faster to fix it in the mould design phase. Trust me, we’ve seen so many clients waste money on post-processing (like sanding or painting over sink marks) when we could’ve fixed it before the mould was even built.

So, to wrap this up: sink marks are those tiny dents on plastic parts caused by uneven cooling and shrinkage of thick areas, and they’re super common, but totally avoidable with good mould design and tweaks to part thickness, packing pressure, cooling, and gates. If you’re working on a plastic product and want to make sure your parts are sink-mark-free, reach out to us to chat through your project. We’re here to help, no BS, just real solutions for your moulding needs.
Plastic Mould References:
- Bralla, J.G. (Ed.). Design for Manufacturability Handbook. McGraw-Hill.
- Rosato, D.V., & Rosato, M.G. (2000). Injection Molding Handbook. Springer.
- plastic Industry Association. (2021). Injection Molding Defect Prevention Guide. National Association of Manufacturers.
Wuxi Santaizi Metal Products Co., Ltd.
As one of the most professional plastic mould manufacturers and suppliers in China, we warmly welcome you to buy high-grade plastic mould made in China here from our factory. All customized metal products are with high quality and competitive price. Contact us for pricelist.
Address: No. 23 Xufeng Road, Xushe Town, Yixing City, Wuxi City, Jiangsu Province, China
E-mail: Ksstzmj@163.com
WebSite: https://www.wuxisantaizi.com/