{"id":652,"date":"2026-11-10T02:17:06","date_gmt":"2026-11-09T18:17:06","guid":{"rendered":"http:\/\/www.ahets.com\/blog\/?p=652"},"modified":"2026-11-10T02:17:06","modified_gmt":"2026-11-09T18:17:06","slug":"what-is-the-sink-mark-in-plastic-products-and-how-to-avoid-it-in-plastic-moulds-404c-278607","status":"publish","type":"post","link":"http:\/\/www.ahets.com\/blog\/2026\/11\/10\/what-is-the-sink-mark-in-plastic-products-and-how-to-avoid-it-in-plastic-moulds-404c-278607\/","title":{"rendered":"What is the sink mark in plastic products and how to avoid it in plastic moulds?"},"content":{"rendered":"<p>Hey everyone, it\u2019s Jake from your go-to plastic mould supplier\u2014today we\u2019re talking about that super annoying thing that ruins even the best-looking plastic parts: sink marks. If you\u2019ve ever picked up a plastic phone case, a toy car, or even a kitchen storage bin and noticed that tiny, dented spot on the back, right where there\u2019s a thick wall inside? That\u2019s a sink mark, and trust me, I\u2019ve gotten so many calls from clients panicking about them. Let\u2019s break this down, no boring textbook jargon (well, maybe a little, but we\u2019ll keep it real), and talk about how we fix them in moulds. <a href=\"https:\/\/www.wuxisantaizi.com\/plastic-mould\/\">Plastic Mould<\/a><\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.wuxisantaizi.com\/uploads\/47927\/small\/high-precision-injection-mold-manufacturingf88ad.jpg\"><\/p>\n<p>First off, let\u2019s keep it simple: what <em>is<\/em> a sink mark, exactly? When you inject molten plastic into a mould, it cools down, right? Thicker areas of the part take longer to cool than thin ones, kind of like how a thick slice of pizza stays hot longer than the crust. As the plastic cools and shrinks, it needs more material to fill in the gaps that form during cooling. If there\u2019s not enough extra plastic (that\u2019s called \u201cpacking pressure\u201d in the mould world) or the cooling happens too fast, the thick spot shrinks inward, leaving that little dimple on the surface. Sometimes it\u2019s barely noticeable, but other times? It\u2019s so bad you can\u2019t ignore it\u2014like a water bottle that has a weird dent right where you grip it, and customers send it back immediately. I once had a client make 5,000 toy action figures that all had sink marks on their thick leg joints, and they had to toss the whole batch. Ouch.<\/p>\n<p>Now, why do sink marks happen in moulds specifically? Let\u2019s get into the nitty-gritty without making your eyes glaze over. Every plastic part has wall thickness\u2014if it\u2019s too uneven, that\u2019s the #1 culprit. A part that\u2019s 2mm thick everywhere is gonna cool evenly, but if one spot is 5mm thick? That\u2019s where the problem starts. Another big one is packing time and pressure. When you shoot plastic into the mould, you don\u2019t just stop when the cavity is full\u2014you hold pressure for a bit to push more molten plastic into the shrinking areas. If you cut that step short, the thick parts can\u2019t get enough material, and boom\u2014sink mark. Also, plastic type matters. Some materials shrink more than others, like ABS vs. polypropylene. PP is super flexible but shrinks a ton, so it\u2019s way more prone to sink marks if you don\u2019t adjust the mould settings.<\/p>\n<p>Here\u2019s the good stuff: how do we <em>avoid<\/em> sink marks in moulds? This is what we do every day at our shop, so these are actual, actionable things, not just theory. First, fix the wall thickness. That\u2019s the easiest (and most effective) fix. If your part has a thick spot, we can add a \u201crib\u201d or a \u201cdraft\u201d to thin it out, or even create a \u201cdead space\u201d inside the thick wall so there\u2019s less material to shrink. For example, if you\u2019re making a plastic gear with a thick hub, instead of making the hub solid, we can hollow it out a little\u2014less material, less shrinkage, no sink mark. We always run simulations (that\u2019s the software we use to test the mould before we build it) to check for thick spots before we even cut steel, which saves clients so much time and money.<\/p>\n<p>Next, adjust the packing and cooling in the mould. This is where we tweak the mould design to control how plastic cools. We add \u201ccooling channels\u201d right next to thick areas\u2014like tiny pipes that run through the mould steel so the plastic cools evenly. If a part has a thick boss (those little cylindrical bumps for screws, super common), we put a cooling line right next to that boss, so it cools at the same rate as the thin areas around it. We also adjust the injection pressure and time: instead of cranking pressure up all at once, we use \u201chold pressure\u201d for a few extra seconds after the cavity is full. That extra pressure pushes more plastic into the shrinking thick areas, so they don\u2019t dip inward.<\/p>\n<p>Another trick we use: \u201cgate design.\u201d Gates are the holes where plastic flows into the mould cavity. If you have a thick part, putting a bigger gate (or multiple smaller gates) right next to the thick area lets more plastic flow there during packing, so it gets the material it needs. I had a client making a plastic remote control\u2014their original gate was tiny, and the back had a big sink mark right over the battery compartment, which is a thick spot. We swapped the gate for a larger one on that side, adjusted the hold time, and all the sink marks were gone. They saved their whole next batch of parts.<\/p>\n<p>Wait, but what if you can\u2019t change the part design? Like, if the client already finalized the part and they can\u2019t thin the walls? We have other hacks. One is \u201cventing.\u201d Adding tiny vents in the mould lets excess air and gas escape when plastic is injected, which helps the plastic flow better and fills gaps in thick areas. Sometimes we also use \u201chot runner\u201d moulds\u2014instead of plastic flowing from a cold sprue, the runner is heated, so plastic stays molten longer. That means more time to pack the thick areas, so less shrinkage. We use hot runners a lot for high-volume parts, like phone cases or appliance parts, because they cut down on waste <em>and<\/em> sink marks.<\/p>\n<p>Let me be real, though\u2014sink marks aren\u2019t always 100% avoidable, but we can get them so small no one notices. Last year, a client came to us with a plastic outdoor table; their old mould had sink marks on the tabletop, and customers were complaining. We redesigned the mould: hollowed out the thick edges of the tabletop, added cooling channels along the edge, and used a hot runner gate. The final parts had almost zero sink marks\u2014you had to hold them up to a light to even see a tiny, unnoticeable spot. The client was stoked, and their return rate dropped by 90%.<\/p>\n<p>Now, why does this matter for you, the person ordering plastic moulds? Because sink marks aren\u2019t just an aesthetic issue\u2014they can weaken the part too. A sink mark is like a tiny dent in the structure; over time, that spot can crack, especially if the part is under stress, like a car panel or a medical device. So fixing sink marks isn\u2019t just about making the part look good\u2014it\u2019s about making it last.<\/p>\n<p>At our mould shop, we don\u2019t just build moulds and send them out. We work with clients from the first design sketch all the way to the final part. If you have a part that\u2019s getting sink marks, or you\u2019re designing a new product and want to avoid them, hit us up. We\u2019ll run those mould simulations for free, suggest tweaks to the design or mould, and make sure your parts come out perfect, no dents, no headaches.<\/p>\n<p>Oh, and one quick pro tip: if you\u2019re dealing with a part that already has a sink mark, sometimes you can fix it after moulding, but it\u2019s way cheaper and faster to fix it in the mould design phase. Trust me, we\u2019ve seen so many clients waste money on post-processing (like sanding or painting over sink marks) when we could\u2019ve fixed it before the mould was even built.<\/p>\n<p><img decoding=\"async\" src=\"https:\/\/www.wuxisantaizi.com\/uploads\/47927\/small\/large-size-plastic-parts92404.jpg\"><\/p>\n<p>So, to wrap this up: sink marks are those tiny dents on plastic parts caused by uneven cooling and shrinkage of thick areas, and they\u2019re super common, but totally avoidable with good mould design and tweaks to part thickness, packing pressure, cooling, and gates. If you\u2019re working on a plastic product and want to make sure your parts are sink-mark-free, reach out to us to chat through your project. We\u2019re here to help, no BS, just real solutions for your moulding needs.<\/p>\n<p><a href=\"https:\/\/www.wuxisantaizi.com\/plastic-mould\/\">Plastic Mould<\/a> References:<\/p>\n<ol>\n<li>Bralla, J.G. (Ed.). <em>Design for Manufacturability Handbook<\/em>. McGraw-Hill.<\/li>\n<li>Rosato, D.V., &amp; Rosato, M.G. (2000). <em>Injection Molding Handbook<\/em>. Springer.<\/li>\n<li>plastic Industry Association. (2021). <em>Injection Molding Defect Prevention Guide<\/em>. National Association of Manufacturers.<\/li>\n<\/ol>\n<hr>\n<p><a href=\"https:\/\/www.wuxisantaizi.com\/\">Wuxi Santaizi Metal Products Co., Ltd.<\/a><br \/>As one of the most professional plastic mould manufacturers and suppliers in China, we warmly welcome you to buy high-grade plastic mould made in China here from our factory. All customized metal products are with high quality and competitive price. Contact us for pricelist.<br \/>Address: No. 23 Xufeng Road, Xushe Town, Yixing City, Wuxi City, Jiangsu Province, China<br \/>E-mail: Ksstzmj@163.com<br \/>WebSite: <a href=\"https:\/\/www.wuxisantaizi.com\/\">https:\/\/www.wuxisantaizi.com\/<\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Hey everyone, it\u2019s Jake from your go-to plastic mould supplier\u2014today we\u2019re talking about that super annoying &hellip; <a title=\"What is the sink mark in plastic products and how to avoid it in plastic moulds?\" class=\"hm-read-more\" href=\"http:\/\/www.ahets.com\/blog\/2026\/11\/10\/what-is-the-sink-mark-in-plastic-products-and-how-to-avoid-it-in-plastic-moulds-404c-278607\/\"><span class=\"screen-reader-text\">What is the sink mark in plastic products and how to avoid it in plastic moulds?<\/span>Read more<\/a><\/p>\n","protected":false},"author":26,"featured_media":652,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1],"tags":[615],"class_list":["post-652","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-industry","tag-plastic-mould-4b96-27ead8"],"_links":{"self":[{"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/posts\/652","targetHints":{"allow":["GET"]}}],"collection":[{"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/users\/26"}],"replies":[{"embeddable":true,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/comments?post=652"}],"version-history":[{"count":0,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/posts\/652\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/posts\/652"}],"wp:attachment":[{"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/media?parent=652"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/categories?post=652"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.ahets.com\/blog\/wp-json\/wp\/v2\/tags?post=652"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}